Why ABS needs an enclosed printer
Print PLA on an open printer and nothing much goes wrong. Swap in ABS and the corners curl, or the part splits up the side halfway through the build. People blame the filament, but it is mostly heat.
It shrinks as it cools
ABS contracts noticeably once it drops below about 100 °C. The layer you just laid is hot, the layers under it are already cooling and pulling inwards, and that tension has nowhere to go. A draft from a window is enough to make one side cool faster than the other, and the part lifts.
An enclosure fixes this by keeping the air around the print warm and still, usually 40–60 °C. Add a bed around 90–110 °C and a nozzle at 230–260 °C and the layers stay fused together. That fusion is what makes ABS tough. Without it you can get a part that looks fine and snaps along a layer line the first time someone loads it.
The smell is real
ABS gives off styrene and fine particles while it prints. If the printer shares a room with people, put it in a closed cabinet and vent or filter the air.
The rule of thumb is simple. ABS, ASA and nylon want an enclosure. PLA and PETG usually do not. And if the part is long, thin and flat, think about ASA or nylon before fighting ABS.